Cause1.Injection pressure or barrel temperature
2.Too much feed material
3.Too long advance time of the pump column
4.Unbalance of the feeding port in multiple writing,
5.There is a depressed part in the mold
6.Deep cylinder parts release vacuum problem
7. Mold opening time change
8.Improper finishing of mold surface
9. Mold core misalignment
Corresponding measures1)Reduce injection pressure or high barrel temperature
2)Reduce feeding material
3)Reduce the advancing time of the service station
4) Limit the flow of plastic, as close as possible to the main stream or single-written mold imbalance of each feed opening
5) Eliminate depressions, lighten or increase the release angle
6) Provide sufficient air escape channels
7)Maintain a fixed mold opening time, if necessary, a timer should be used
8)Lighten the surface of the mold writing
9)Adjust the mold center and lock it by using the withdrawal angle.
Latest blog posts
Custom molds injection molding
Custom molds injection molding is a manufacturing process that involves creating custom molds to produce plastic parts. Injection molding is a popular technique used in various industries such as...
Plastic injection molding companies
Plastic injection molding is a manufacturing process that involves injecting molten plastic into a mold to create a wide range of plastic products. From car parts to medical devices and household items, plastic injection molding is used to create a variet
PET Preform Injection Moulding Machine
PET preform injection molding is a manufacturing process that is used to create PET (polyethylene terephthalate) preforms that can be later blown into bottles, jars, and other containers. This process...
You may like
Analysis of the causes of unstable color of injection molded shell parts
Now, the application of plastic shell has been widely up, life, we are very common, such as: electrical shells, and our usual washbasin, all belong to the plastic, but in...
Process tips for shrinkage problems of thick-walled injection molded parts
The shrinkage problem of plastic parts (surface shrinkage and internal shrinkage) is caused by the defect of insufficient melt replenishment when the thicker parts are cooled. We...
Injection parameters and control
Temperature,Temperature measurement and control are very important in injection molding. Although it is relatively simple to make these measurements, most injection molding machines do not have adequate pick points or lines...
How to increase the brightness of injection molded products from process and mold?
I. Injection mold, 1). If the mold cavity processing is poor, such as scars, microporous, wear, roughness, and other deficiencies, will inevitably react to the plastic parts...