What is the main flow channel sticking to the mold (appearance)
Main runner residue is a phenomenon that the main runner of molded products fails to break away from the mold.
If the main runner size increases due to long-time pressure-holding, or if the main runner part of the mold is injured, resistance will be generated so that the main runner cannot come off when the mold is opened.
Main flow channel sticky mold generation causes
1、Mainstream channel curing is not sufficient
When the main channel has not been fully cured, due to the shrinkage at this moment being very small, the main channel close to the mold, the strength is also low, so if at this time to make the main channel out, it will be very easy to break. In this way, the main flow channel will be left behind. Resin temperature, mold temperature, and cycle (cooling time) on the mainstream channel curing have an impact.
2、Over-application of holding pressure
The main runner section is closest to the barrel nozzle, so it is easy to apply to hold pressure. Therefore, after applying high holding pressure, the size of the main flow channel will increase, and the resistance of the mold release will also increase accordingly so that the main flow channel is prone to sticky mold.
3、The problem of the mold structure
When the slope of the main flow channel is small, the resistance of the fixed side will increase. Although the main runner is locked to pull out the main runner from the fixed side, if it is weak, the lock will be damaged and the main runner will fall off from the mobile side. Also, if a manifold lock is used, because it is too strong, the main flow channel and manifold sometimes adhere to the fixed side.
4. Problems inherent in the grade
Compared with the standard grade, the impact resistance grade or alloy material shrinks less and adheres to the mold more easily and with lower strength. This makes it easier for the mainstream channel to stick to the mold.
Countermeasures for mold sticking in the main channel
1. Allow the main channel to cool and cure sufficiently before opening the mold
Reduce the mold temperature and extend the cooling time. Especially for the material with low strength and slow curing, lowering the mold temperature will be an effective method.
2、Lower the holding pressure
Reducing the holding pressure is also effective. The holding pressure applied to the product cavity will become zero after the gate is closed, so if no holding pressure is applied thereafter, the main flow path will not be subjected to useless holding pressure. However, the excessive reduction will easily lead to unstable injection volume, so care is needed.
3、 Improve the mold
The angle necessary for the slope of the main flow channel has not yet been specifically defined. However, if there is a possibility of mold sticking in the main channel, increasing the angle can be effective. Strengthening the main runner lock (increasing the size and enhancing the slope) is also effective. On the contrary, since it may become difficult to come off due to ejection, it needs to be adjusted while molding.
If the manifold lock is too strong, change the size of this part slightly.
Last: Four kinds of mold surface treatment technology Next: 88 mold design common basic knowledge
Latest blog posts
Custom molds injection molding
Custom molds injection molding is a manufacturing process that involves creating custom molds to produce plastic parts. Injection molding is a popular technique used in various industries such as...
Plastic injection molding companies
Plastic injection molding is a manufacturing process that involves injecting molten plastic into a mold to create a wide range of plastic products. From car parts to medical devices and household items, plastic injection molding is used to create a variet
PET Preform Injection Moulding Machine
PET preform injection molding is a manufacturing process that is used to create PET (polyethylene terephthalate) preforms that can be later blown into bottles, jars, and other containers. This process...
You may like
Four kinds of mold surface treatment technology
In the work of the mold, in addition to the requirement of the substrate to have a high enough strength and toughness of a reasonable fit, its surface properties are essential to the working performance...
Twelve kinds of injection molding defect cause 360 degree depth perfect analysis
I. Analysis of the causes of cracking of injection molded products
Cracking, including the surface of the parts filamentary cracks, microcrack, top white, cracking and caused...
Child safety seat injection molding and blow molding process of the 4 major differences
Plastic parts are a large part of the child safety seat, the quality of the plastic parts determines whether they will break in the event of an accident. Child seat plastic...
5 general plastic injection molding process details
Polypropylene (PP) injection mold processing technology,PP is a transparent, semi-crystalline thermosetting plastic with high toughness, good dielectric strength, low water absorption, high thermal deformation temperature...