1) Inconsistent molding conditions or improper operation
When injection molding, the temperature, pressure and time, and other process parameters must be strictly controlled in accordance with the process requirements, especially the molding cycle of each plastic part must be consistent, not arbitrary changes. If the injection pressure is too low, the holding time is too short, the mold temperature is too low or uneven, the temperature at the barrel and nozzle is too high, and the cooling of the plastic part is not enough, it will lead to the unstable size of the plastic part.
In general, the use of higher injection pressure and injection speed, the appropriate extension of the mold filling and holding time, improve the mold temperature and material temperature, is conducive to overcoming the size instability failure.
If the size of the molded part is larger than the required size, the injection pressure and melt temperature should be reduced, the mold temperature should be increased, the mold filling time should be shortened, and the gate cross-sectional area should be reduced to increase the shrinkage rate of the molded part.
If the size of the molded part is smaller than the required size, the opposite molding conditions should be adopted.
It is worth noting that the change of ambient temperature also has a certain influence on the fluctuation of molding size of plastic parts, and the process temperature of equipment and mold should be adjusted timely according to the change of external environment.
2) Improper selection of molding raw materials
The shrinkage rate of molding raw materials has a great impact on the dimensional accuracy of plastic parts. If the precision of molding equipment and molds is high, but the shrinkage rate of molding raw materials is large, it is difficult to ensure the dimensional accuracy of plastic parts. Generally speaking, the larger the shrinkage rate of molding materials, the more difficult it is to ensure the dimensional accuracy of plastic parts. Therefore, the selection of molding resin must be fully considered after the shrinkage of raw materials molding on the impact of dimensional accuracy of plastic parts. For the choice of raw materials, the shrinkage rate of the range of change can not be greater than the requirements of the dimensional accuracy of the plastic parts.
It should be noted that the shrinkage rate of various resins varies greatly and is analyzed according to the degree of crystallization of the resin. Usually, the shrinkage rate of crystalline and semi-crystalline resins is larger than that of non-crystalline resins, and the range of change in shrinkage rate is also larger, and the shrinkage rate fluctuates more after the molding of the corresponding plastic parts; for crystalline resins, the crystallinity is high, the molecular volume shrinks, and the shrinkage of the plastic parts is large; the size of the resin spherical crystal also has an impact on the shrinkage rate, and the spherical crystal is small, and the space between molecules is small, and the shrinkage of the plastic parts is smaller, while the Impact strength is higher.
In addition, if the molding of raw materials of uneven particle size, poor drying, uneven mixing of recycled materials and new materials, the performance of each batch of raw materials is different, will also cause fluctuations in the molding size of plastic parts.
3) Mold failure
The structural design and manufacturing accuracy of the mold directly affects the dimensional accuracy of the plastic parts. In the molding process, if the rigidity of the mold is insufficient or the molding pressure inside the mold cavity is too high to deform the mold, the liver will cause the molding size of the plastic parts to be unstable.
If the clearance between the guide pillar and guide bush of the mold is poor due to poor manufacturing accuracy or too much wear and tear, it will also make the molding dimensional accuracy of the plastic parts decrease.
If there is hard filler or glass fiber reinforced material in the molding raw material which leads to serious wear of the mold cavity, or when using a mold with multiple cavities, there are errors between the cavities and gates, runners and other errors and poor balance of the inlet and other reasons to produce inconsistent mold filling will also cause size fluctuations.
Therefore, in the design of the mold, should design sufficient mold strength and rigidity, strict control of processing accuracy, mold cavity materials should use wear-resistant materials, cavity surface heat treatment, and cold hardening treatment is best. When the dimensional accuracy of the plastic part is very high, it is better not to adopt the structure form of one mold with multiple cavities, otherwise, in order to ensure the molding accuracy of the plastic part, a series of auxiliary devices must be set on the mold to ensure the accuracy of the mold, which leads to the high production cost of the mold.
When the plastic part has the error of partial thickness, it is often also caused by mold failure. If the wall thickness of the plastic part under the condition of one mold and one cavity produces deviated thickness error, it is generally due to the installation error of the mold and poor positioning which causes the relative position of the mold cavity and the core to be shifted.
At this time, for those wall thickness size requirements are very accurate plastic parts, can not rely only on the guide pillar and guide bush to position, must be added to other positioning devices; If it is in a mold under the conditions of multiple cavities generated by the thickness error, in general, the molding error is small at the beginning, but the error gradually becomes larger after the continuous operation, which is mainly due to the error between the cavity and the core, especially when using hot runner mold molding is most likely to produce this phenomenon. This is mainly due to the error between the cavity and the core, especially when the hot runner mold is used. In this regard, a double cooling circuit with a small temperature difference can be set up in the mold. In the case of forming thin-walled round containers, a floating core can be used, but the core and cavity must be concentric.
In addition, in the production of the mold, in order to facilitate the repair of the mold, it is always customary to make the cavity smaller than the required size, the core to make a larger than the required size, leaving a certain amount of repair margin. When the inner diameter of the molding hole is smaller than the outer diameter, the core pin should be made larger, which is due to the shrinkage of the molding hole being always larger than other parts, and shrinkage to the direction of the hole center. On the contrary, if the inner diameter of the molding hole is close to the outer diameter, the core pin can be made smaller.
4) Equipment failure
If the plasticizing capacity of the
molding equipment is insufficient, the feeding system is unstable, the rotational speed of the screw is unstable, the stopping action is out of order, the check valve of the hydraulic system is out of order, the thermocouple of the temperature control system is burnt out, the heater is disconnected, etc., it will lead to the unstable molding size of the plastic parts. These faults can be eliminated by taking targeted measures as long as they are identified.
5) Inconsistent test methods or conditions
If the method, time, and temperature of measuring the size of plastic parts are different, the measured size will be very different. Among them, the temperature conditions have the greatest impact on the test, which is because the coefficient of thermal expansion of plastic is 10 times greater than that of the metal industry. Therefore, it is necessary to use the standard method and temperature conditions to determine the structural dimensions of the plastic part, and the plastic part must be sufficiently cooled and set before measurement. Generally, the dimensional change of the plastic part is very large within 10 hours of demoulding, and only after 24 hours is it basically set.
Latest blog posts
Custom molds injection molding
Custom molds injection molding is a manufacturing process that involves creating custom molds to produce plastic parts. Injection molding is a popular technique used in various industries such as...
Plastic injection molding companies
Plastic injection molding is a manufacturing process that involves injecting molten plastic into a mold to create a wide range of plastic products. From car parts to medical devices and household items, plastic injection molding is used to create a variet
PET Preform Injection Moulding Machine
PET preform injection molding is a manufacturing process that is used to create PET (polyethylene terephthalate) preforms that can be later blown into bottles, jars, and other containers. This process...
You may like
The process principle and requirements of high gloss injection molding
The process principle of high gloss injection molding.The mold is heated up before and during the mold closing process, and after the mold closing is completed, the temperature reaches the set...
Causes of glow lines in the gate area of injection molded products
In the design of the point gate in the vertical direction of the part, a radiation system consisting of different color depths and luster, called glow lines, appears on the surface of the part during injection molding...
How to repair the injection molding machine?
Introduction: Injection molding machine is also known as injection molding machine or injection machine. It is the main molding equipment to make thermoplastic or thermosetting plastic...
Why is it important to maintain PET bottle blanks for injection moulds?
The maintenance of plastic bottle cap moulds is a useful measure to ensure the normal operation of the injection moulds. The maintenance of the equipment mainly includes finishing...